{"id":20068,"date":"2026-11-06T15:30:19","date_gmt":"2026-11-06T15:30:19","guid":{"rendered":"https:\/\/az-broquetas.es\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau"},"modified":"2026-11-06T15:41:54","modified_gmt":"2026-11-06T15:41:54","slug":"diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","status":"publish","type":"post","link":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","title":{"rendered":"Difer\u00e8ncies entre l&#8217;acer inoxidable AISI 304 i l&#8217;AISI 316L: quan triar cada grau"},"content":{"rendered":"\n<p class=\"wp-block-paragraph\">En una xarxa interior d&#8217;aigua freda potable, amb aigua de composici\u00f3 ordin\u00e0ria i una refer\u00e8ncia certificada, <strong>l&#8217;AISI 304 acostuma a ser suficient<\/strong>. L&#8217;AISI 316L aporta un marge addicional quan augmenten els clorurs, la temperatura o l&#8217;exposici\u00f3 exterior a sals, i quan la documentaci\u00f3 del producte o l&#8217;enginyeria del projecte ho prescriu.<\/p>\n\n<p class=\"wp-block-paragraph\">En aigua calenta sanit\u00e0ria, la temperatura canvia l&#8217;an\u00e0lisi. Una xarxa que treballa per sobre de 50\u201360 \u00b0C <strong>no s&#8217;ha d&#8217;avaluar amb els mateixos rangs orientatius<\/strong> que una xarxa d&#8217;aigua freda. S&#8217;han de considerar conjuntament clorurs, oxidants, estancament, escletxes, tensions i tractaments t\u00e8rmics.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Ni l&#8217;aerot\u00e8rmia ni el glicol determinen per si sols el grau<\/strong>. En aquestes aplicacions s&#8217;han de comprovar la composici\u00f3 i el manteniment del fluid, l&#8217;ambient, la temperatura, les unions i els l\u00edmits del sistema complet.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Resposta r\u00e0pida: orientaci\u00f3 inicial per a l&#8217;instal\u00b7lador<\/strong><\/h2>\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>Situaci\u00f3<\/strong><\/td><td><strong>Orientaci\u00f3 inicial<\/strong><\/td><td><strong>Condicions que s&#8217;han de comprovar<\/strong><\/td><\/tr><tr><td>Aigua freda potable interior<\/td><td>Una refer\u00e8ncia certificada en AISI 304 acostuma a ser suficient.<\/td><td>Composici\u00f3 de l&#8217;aigua, temperatura ambient, circulaci\u00f3 i abs\u00e8ncia d&#8217;exposici\u00f3 salina.<\/td><\/tr><tr><td>ACS<\/td><td>No extrapolar els rangs d&#8217;aigua freda; el 316L pot aportar marge.<\/td><td>Temperatura normal i m\u00e0xima, clorurs, oxidants, estancament, tensions i tractaments t\u00e8rmics.<\/td><\/tr><tr><td>Clorurs elevats o sals exteriors<\/td><td>L&#8217;AISI 316L aporta un marge m\u00e9s gran, dins dels seus l\u00edmits.<\/td><td>Clorurs, temperatura, oxidants, dip\u00f2sits, escletxes, neteja i acabat.<\/td><\/tr><tr><td>Aerot\u00e8rmia o glicol<\/td><td>L&#8217;AISI 304 pot ser suficient en condicions controlades; el 316L aporta marge si augmenta la severitat.<\/td><td>Fitxa del fluid, aigua de mescla, temperatura, manteniment i exposici\u00f3 exterior.<\/td><\/tr><tr><td>Unions soldades<\/td><td>Especificar 304L o 316L segons el medi i executar correctament.<\/td><td>Procediment, protecci\u00f3 de l&#8217;arrel, contaminaci\u00f3 i neteja de la coloraci\u00f3 t\u00e8rmica.<\/td><\/tr><tr><td>Aigua de mar<\/td><td>No prescriure AISI 304 ni AISI 316L de forma gen\u00e8rica.<\/td><td>Selecci\u00f3 espec\u00edfica d&#8217;aliatge, disseny, escletxes, dip\u00f2sits, circulaci\u00f3 i temperatura.<\/td><\/tr><\/tbody><\/table><\/figure>\n\n<p class=\"wp-block-paragraph\"><strong>La taula ofereix una orientaci\u00f3 inicial.<\/strong> Quan l&#8217;aigua, l&#8217;ambient o el proc\u00e9s se situen a prop dels l\u00edmits del material, ha de prevaldre la documentaci\u00f3 de la refer\u00e8ncia concreta i el criteri del projectista.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Qu\u00e8 diferencia realment l&#8217;AISI 304 de l&#8217;AISI 316L<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">Tots dos s\u00f3n acers inoxidables austen\u00edtics. La seva resist\u00e8ncia a la corrosi\u00f3 es basa en una capa passiva rica en \u00f2xid de crom que es forma sobre la superf\u00edcie.<\/p>\n\n<p class=\"wp-block-paragraph\">L&#8217;AISI 316L cont\u00e9 molibd\u00e8; l&#8217;AISI 304 no l&#8217;incorpora deliberadament com a element d&#8217;aliatge. <strong>El molibd\u00e8 millora la resist\u00e8ncia relativa<\/strong> a la corrosi\u00f3 per picadures i en escletxes en nombrosos medis amb clorurs.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>El comportament real no dep\u00e8n \u00fanicament del grau<\/strong>. La temperatura, els oxidants, l&#8217;acabat superficial, les soldadures, l&#8217;estancament, els dip\u00f2sits, les tensions i la geometria poden reduir el marge disponible.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Composici\u00f3 qu\u00edmica de refer\u00e8ncia<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">La seg\u00fcent composici\u00f3 correspon a les designacions europees 1.4301 i 1.4404 segons EN 10088. Per a un producte concret s&#8217;ha de consultar el certificat de material.<\/p>\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>Element<\/strong><\/td><td><strong>1.4301 \/ AISI 304<\/strong><\/td><td><strong>1.4404 \/ AISI 316L<\/strong><\/td><\/tr><tr><td>Crom (Cr)<\/td><td>17,0\u201319,5 %<\/td><td>16,5\u201318,5 %<\/td><\/tr><tr><td>N\u00edquel (Ni)<\/td><td>8,0\u201310,5 %<\/td><td>10,0\u201313,0 %<\/td><\/tr><tr><td>Molibd\u00e8 (Mo)<\/td><td>No afegit deliberadament<\/td><td>2,0\u20132,5 %<\/td><\/tr><tr><td>Carboni (C), m\u00e0xim<\/td><td>0,07 %<\/td><td>0,030 %<\/td><\/tr><tr><td>Mangan\u00e8s (Mn), m\u00e0xim<\/td><td>2,0 %<\/td><td>2,0 %<\/td><\/tr><tr><td>Nitrogen (N), m\u00e0xim<\/td><td>0,11 %<\/td><td>0,11 %<\/td><\/tr><\/tbody><\/table><\/figure>\n\n<p class=\"wp-block-paragraph\">El nitrogen s&#8217;inclou perqu\u00e8 forma part de la f\u00f3rmula del PREN. Els intervals poden canviar si s&#8217;utilitza una altra norma o una designaci\u00f3 diferent.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>El PREN: un \u00edndex comparatiu, no un percentatge de resist\u00e8ncia<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">El PREN \u2014Pitting Resistance Equivalent Number\u2014 permet comparar la resist\u00e8ncia relativa a la picadura a partir de la composici\u00f3 qu\u00edmica. Una expressi\u00f3 habitual \u00e9s:<\/p>\n\n<p class=\"wp-block-paragraph\">PREN = %Cr + 3,3 \u00d7 %Mo + 16 \u00d7 %N<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Amb composicions nominals, l&#8217;AISI 304 se situa habitualment al voltant de 18\u201320 i l&#8217;AISI 316L al voltant de 24\u201326.<\/strong> Un PREN m\u00e9s alt no significa que el material hagi de durar un percentatge concret m\u00e9s ni defineix una concentraci\u00f3 m\u00e0xima universal de clorurs.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>CPT i CCT: la temperatura tamb\u00e9 forma part del problema<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">La temperatura cr\u00edtica de picadura \u2014CPT\u2014 i la temperatura cr\u00edtica de corrosi\u00f3 en escletxes \u2014CCT\u2014 permeten comparar aliatges mitjan\u00e7ant assajos accelerats. <a href=\"https:\/\/store.astm.org\/standards\/g48\">ASTM G48<\/a> preveu m\u00e8todes per determinar CPT i CCT en una soluci\u00f3 normalitzada de clorur f\u00e8rric; <a href=\"https:\/\/store.astm.org\/standards\/g150\">ASTM G150<\/a> determina electroqu\u00edmicament la CPT.<\/p>\n\n<p class=\"wp-block-paragraph\">Aquests valors serveixen per ordenar materials i controlar productes, no per traslladar directament una temperatura de laboratori a una instal\u00b7laci\u00f3. ASTM adverteix que les condicions d&#8217;assaig acceleren la corrosi\u00f3 i no simulen un entorn real de servei. El concepte s\u00ed que aporta una conclusi\u00f3 pr\u00e0ctica: dues aig\u00fces amb els mateixos clorurs poden plantejar riscos diferents si treballen a temperatures diferents.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Qu\u00e8 significa la \u00abL\u00bb de 316L<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>La \u00abL\u00bb identifica una variant de baix carboni.<\/strong> En el 316L, el carboni es limita a un m\u00e0xim del 0,030 %. Aix\u00f2 redueix el risc de sensibilitzaci\u00f3 a les zones afectades t\u00e8rmicament durant la soldadura.<\/p>\n\n<p class=\"wp-block-paragraph\">En una instal\u00b7laci\u00f3 soldada, la comparaci\u00f3 no sempre s&#8217;ha de plantejar entre 304 i 316L. Existeix tamb\u00e9 el 304L. <strong>La selecci\u00f3 ha de considerar<\/strong> el grau d&#8217;aliatge, la variant de baix carboni, el procediment de soldadura, la protecci\u00f3 de l&#8217;arrel i la neteja posterior.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Les difer\u00e8ncies que s\u00ed que s\u00f3n comparables<\/strong><\/h2>\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>Caracter\u00edstica<\/strong><\/td><td><strong>AISI 304<\/strong><\/td><td><strong>AISI 316L<\/strong><\/td><\/tr><tr><td>Molibd\u00e8<\/td><td>No afegit deliberadament<\/td><td>2,0\u20132,5 % segons EN 10088 per a 1.4404<\/td><\/tr><tr><td>PREN orientatiu<\/td><td>Aproximadament 18\u201320<\/td><td>Aproximadament 24\u201326<\/td><\/tr><tr><td>Picadura i escletxes amb clorurs<\/td><td>Menor resist\u00e8ncia relativa<\/td><td>Major resist\u00e8ncia relativa, sense immunitat<\/td><\/tr><tr><td>Carboni i soldadura<\/td><td>Valorar 304L si es solda<\/td><td>El baix carboni redueix el risc de sensibilitzaci\u00f3<\/td><\/tr><\/tbody><\/table><\/figure>\n\n<h2 class=\"wp-block-heading\"><strong>Clorurs, cloraci\u00f3 i duresa: tres conceptes diferents<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>Els clorurs s\u00f3n ions presents a l&#8217;aigua.<\/strong> Poden procedir de l&#8217;origen del subministrament, la intrusi\u00f3 salina, un proc\u00e9s industrial o una contaminaci\u00f3. El seu efecte dep\u00e8n especialment de la concentraci\u00f3 i la temperatura, per\u00f2 tamb\u00e9 de les escletxes, els dip\u00f2sits, l&#8217;estancament i les soldadures.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>La cloraci\u00f3 \u00e9s un tractament de desinfecci\u00f3 mitjan\u00e7ant subst\u00e0ncies oxidants.<\/strong> El clor lliure residual i la concentraci\u00f3 d&#8217;ions clorur s\u00f3n par\u00e0metres diferents. Tots dos poden influir en la corrosi\u00f3, per\u00f2 s&#8217;han de mesurar per separat.<\/p>\n\n<p class=\"wp-block-paragraph\">La duresa expressa principalment el contingut de calci i magnesi. Pot afavorir incrustacions, per\u00f2 no permet decidir per si sola entre AISI 304 i AISI 316L.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Orientaci\u00f3 quantitativa per a aigua natural a temperatura ambient<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">La guia <a href=\"https:\/\/nickelinstitute.org\/media\/jbmlp0cs\/11019_stainlesssteelplumbing.pdf\">Stainless Steel Plumbing del Nickel Institute<\/a> recull, com a refer\u00e8ncia d&#8217;experi\u00e8ncia en aigua natural en circulaci\u00f3 i a temperatura ambient, que la picadura i la corrosi\u00f3 en escletxes del 304 s\u00f3n poc freq\u00fcents fins a aproximadament 200 ppm de clorurs, i les del 316 fins a aproximadament 1.000 ppm.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Aquests valors s\u00f3n orientatius, no l\u00edmits de disseny.<\/strong> No s&#8217;han d&#8217;aplicar sense correcci\u00f3 a aigua calenta, ACS, trams estancats, superf\u00edcies amb dip\u00f2sits, escletxes, soldadures sense netejar o sistemes amb oxidants elevats.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Per sota d&#8217;aquests rangs no existeix una garantia autom\u00e0tica d&#8217;abs\u00e8ncia de corrosi\u00f3.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Per sobre d&#8217;ells no es pot decidir el material sense estudiar el conjunt de condicions.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 La fitxa t\u00e8cnica, la certificaci\u00f3 i les limitacions del fabricant prevalen sobre una xifra gen\u00e8rica.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 En aigua de consum s&#8217;ha de verificar la conformitat sanit\u00e0ria del producte complet.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Aigua freda i ACS no s\u00f3n el mateix escenari<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>En aigua freda interior, la temperatura acostuma a proporcionar un marge m\u00e9s gran davant la corrosi\u00f3 localitzada i la fissuraci\u00f3 per clorurs.<\/strong> En ACS, el material treballa habitualment a temperatures m\u00e9s elevades i pot experimentar per\u00edodes d&#8217;estancament, dip\u00f2sits i tractaments t\u00e8rmics.<\/p>\n\n<p class=\"wp-block-paragraph\">El <a href=\"https:\/\/www.boe.es\/eli\/es\/rd\/2022\/06\/21\/487\/con\">Real Decreto 487\/2022<\/a> estableix per a determinades instal\u00b7lacions d&#8217;ACS temperatures m\u00ednimes de 60 \u00b0C en acumulaci\u00f3 i permet arribar a 70 \u00b0C en tractaments t\u00e8rmics. Aquestes temperatures no provoquen corrosi\u00f3 per si mateixes, per\u00f2 obligen a revisar els clorurs, els oxidants, les tensions, les unions i l&#8217;estat superficial amb m\u00e9s atenci\u00f3.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>No s&#8217;ha d&#8217;extrapolar a ACS<\/strong> el rang orientatiu de clorurs publicat per a aigua natural en circulaci\u00f3 a temperatura ambient. La documentaci\u00f3 del sistema, l&#8217;an\u00e0lisi de l&#8217;aigua i les temperatures reals han de governar la selecci\u00f3.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Corrosi\u00f3 sota tensi\u00f3 per clorurs: el l\u00edmit que el molibd\u00e8 no elimina<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">La fissuraci\u00f3 per corrosi\u00f3 sota tensi\u00f3 per clorurs \u2014chloride stress corrosion cracking o CSCC\u2014 requereix la coincid\u00e8ncia d&#8217;un medi amb clorurs, tensions de tracci\u00f3 i condicions t\u00e8rmiques favorables. Les tensions poden procedir del servei, del conformat o de la soldadura.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>En solucions aproximadament neutres i amb immersi\u00f3 completa, aquest mecanisme \u00e9s poc habitual per sota d&#8217;uns 50 \u00b0C.<\/strong> No \u00e9s un llindar universal: quan els clorurs es concentren per evaporaci\u00f3 o per cicles de mullat i secat pot apar\u00e8ixer a temperatures inferiors.<\/p>\n\n<p class=\"wp-block-paragraph\">El molibd\u00e8 del 316L millora la resist\u00e8ncia relativa a la picadura i a la corrosi\u00f3 en escletxes, per\u00f2 <strong>no elimina la susceptibilitat<\/strong> dels inoxidables austen\u00edtics a la fissuraci\u00f3 per clorurs. Si el risc \u00e9s significatiu poden ser necessaris canvis de disseny, barreres davant la humitat, reducci\u00f3 de tensions o graus m\u00e9s resistents.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Corrosi\u00f3 sota a\u00efllament: per qu\u00e8 importa la humitat<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">Sota un a\u00efllament humit, l&#8217;aigua pot extreure sals solubles del propi a\u00efllament o de l&#8217;ambient i transportar-les fins a la superf\u00edcie met\u00e0l\u00b7lica. Els cicles t\u00e8rmics concentren aquestes sals en evaporar-se l&#8217;aigua. Si a m\u00e9s existeixen tensions de tracci\u00f3, es crea un escenari favorable per a la fissuraci\u00f3 per clorurs.<\/p>\n\n<p class=\"wp-block-paragraph\">La inspecci\u00f3 s&#8217;ha de centrar en juntes del revestiment, penetracions, punts baixos, suports i zones on pugui entrar o acumular-se aigua. La barrera exterior, el segellat i la possibilitat de drenatge formen part de la prevenci\u00f3.<\/p>\n\n<p class=\"wp-block-paragraph\">La <a href=\"https:\/\/www.une.org\/encuentra-tu-norma\/busca-tu-norma?k=%28i%3A9110060%29\">UNE-EN ISO 12624:2023<\/a> estableix el m\u00e8tode per determinar traces de clorurs, fluorurs, silicats i sodi solubles en aigua, a m\u00e9s del pH, en productes a\u00efllants t\u00e8rmics. \u00c9s un m\u00e8tode d&#8217;assaig; no estableix per si sol un l\u00edmit universal d&#8217;acceptaci\u00f3 per a cada instal\u00b7laci\u00f3.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>En productes solars o t\u00e8rmics a\u00efllats, una temperatura m\u00e0xima de servei del conjunt no demostra per si sola que existeixi risc.<\/strong> Han de coincidir humitat, sals solubles, tensions i una temperatura superficial desfavorable.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Aigua de mar i ambients costaners<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">L&#8217;aigua de mar cont\u00e9 una concentraci\u00f3 de clorurs molt superior a la d&#8217;una xarxa d&#8217;aigua potable. L&#8217;AISI 316L pot patir picadures i corrosi\u00f3 en escletxes, especialment amb dip\u00f2sits o estancament. <strong>No s&#8217;ha de prescriure com a soluci\u00f3 universal<\/strong> per a conducci\u00f3 d&#8217;aigua de mar.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Un ambient costaner \u00e9s diferent.<\/strong> A l&#8217;exterior poden dipositar-se aerosols salins i concentrar-se durant els cicles d&#8217;humectaci\u00f3 i secat. El 316L aporta m\u00e9s marge que el 304, per\u00f2 la decisi\u00f3 dep\u00e8n de l&#8217;exposici\u00f3, la temperatura, l&#8217;a\u00efllament, la neteja i les escletxes.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Quan acostuma a ser suficient l&#8217;AISI 304<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">Una refer\u00e8ncia certificada en AISI 304 acostuma a ser raonable en xarxes interiors d&#8217;aigua freda potable quan l&#8217;an\u00e0lisi de l&#8217;aigua i la temperatura s\u00f3n compatibles amb la documentaci\u00f3, la instal\u00b7laci\u00f3 est\u00e0 protegida de sals exteriors i les unions s&#8217;executen segons les instruccions del sistema.<\/p>\n\n<p class=\"wp-block-paragraph\">Tamb\u00e9 es pot utilitzar en circuits tancats i altres aplicacions quan el fabricant confirma la compatibilitat amb el fluid i les condicions de treball.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Quan aporta marge addicional l&#8217;AISI 316L<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>L&#8217;AISI 316L pot aportar marge<\/strong> davant la corrosi\u00f3 localitzada quan augmenten els clorurs dins d&#8217;un rang compatible, existeix exposici\u00f3 exterior a sals, puja la temperatura o l&#8217;especificaci\u00f3 t\u00e8cnica exigeix 316L.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Aquest marge no equival a immunitat davant de picadures, corrosi\u00f3 en escletxes o fissuraci\u00f3 per clorurs.<\/strong> Si les condicions superen la seva capacitat poden requerir-se graus m\u00e9s aliats, acers d\u00faplex o altres materials.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Aerot\u00e8rmia i glicol: l&#8217;aplicaci\u00f3 no decideix l&#8217;acer<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>En un circuit interior d&#8217;aerot\u00e8rmia, tancat, amb fluid controlat i una refer\u00e8ncia certificada, el 304 pot ser suficient.<\/strong> El 316L aporta marge quan concorren clorurs, exposici\u00f3 exterior a sals, temperatures m\u00e9s exigents o una prescripci\u00f3 espec\u00edfica.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Un glicol correctament formulat i inhibit tampoc obliga autom\u00e0ticament a utilitzar 316L.<\/strong> S&#8217;han de consultar la fitxa del fluid, l&#8217;aigua de mescla, la temperatura i la documentaci\u00f3 del sistema. El manteniment es desenvolupa a <a href=\"https:\/\/az-broquetas.es\/ca\/canonada-per-a-aerotermia-i-solar-termica-que-exigeix-la-installacio-al-material\">Tuber\u00eda para aerotermia y solar t\u00e9rmica: condiciones de servicio y criterios de selecci\u00f3n<\/a>.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Soldadura i acabat: el material no compensa una execuci\u00f3 deficient<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">Per conservar la resist\u00e8ncia a la corrosi\u00f3 s&#8217;han de controlar el procediment, la protecci\u00f3 de l&#8217;arrel, l&#8217;aportaci\u00f3, la contaminaci\u00f3 per acer al carboni i la neteja de la coloraci\u00f3 t\u00e8rmica.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Una zona soldada mal protegida es pot convertir en el punt m\u00e9s feble fins i tot amb AISI 316L.<\/strong> En instal\u00b7lacions soldades conv\u00e9 especificar variants de baix carboni \u2014304L o 316L\u2014 i un procediment compatible amb el servei.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Conformitat sanit\u00e0ria en aigua de consum<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">L&#8217;article 44 del <a href=\"https:\/\/www.boe.es\/buscar\/act.php?id=BOE-A-2023-628\">Real Decreto 3\/2023<\/a> exigeix que els materials i productes en contacte amb aigua de consum no n&#8217;empitjorin la qualitat ni transmetin subst\u00e0ncies, g\u00e8rmens o propietats perjudicials. Els operadors i empreses constructores han de verificar pr\u00e8viament que els productes compleixen els requisits aplicables.<\/p>\n\n<p class=\"wp-block-paragraph\">L&#8217;annex IX estableix criteris per a materials met\u00e0l\u00b7lics, inclosa la utilitzaci\u00f3 de composicions admeses i les proves corresponents. Per aix\u00f2, especificar \u00abAISI 304\u00bb o \u00abAISI 316L\u00bb no n&#8217;hi ha prou: <strong>s&#8217;ha de comprovar la conformitat del producte complet<\/strong>, inclosos tub, r\u00e0cords, juntes i la resta de components en contacte amb l&#8217;aigua.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Com aplica el sistema CATS aquests criteris<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\"><strong>AZ Broquetas publica configuracions CATS en AISI 304 i AISI 316L segons la refer\u00e8ncia i l&#8217;aplicaci\u00f3.<\/strong> La informaci\u00f3 p\u00fablica indica AISI 316L per a gas i AISI 304 o AISI 316L per a determinades aplicacions d&#8217;aigua potable.<\/p>\n\n<p class=\"wp-block-paragraph\">Abans de prescriure una refer\u00e8ncia s&#8217;han de comprovar el fluid autoritzat, di\u00e0metre, pressi\u00f3, temperatura, r\u00e0cords, juntes, certificaci\u00f3, ambient i instruccions de muntatge.<\/p>\n\n<p class=\"wp-block-paragraph\"><strong>Les dades actualitzades es troben a<\/strong> <a href=\"https:\/\/az-broquetas.es\/caracteristicas-tubo-corrugado-inox\"><strong>Caracter\u00edstiques del tub corrugat inox sistema CATS<\/strong><\/a><strong>.<\/strong> Per comparar el corrugat amb una soluci\u00f3 r\u00edgida es pot consultar <a href=\"https:\/\/az-broquetas.es\/ca\/tub-corrugat-inox-enfront-de-coure-taula-comparativa-tecnica\">Tubo corrugado inox frente a cobre: diferencias t\u00e9cnicas y criterios de elecci\u00f3n<\/a>.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Llista de comprovaci\u00f3 abans de seleccionar 304 o 316L<\/strong><\/h2>\n\n<p class=\"wp-block-paragraph\">\u2022 Designaci\u00f3 exacta i norma del material.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Certificaci\u00f3 de la refer\u00e8ncia per al fluid i l&#8217;aplicaci\u00f3.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Diferenciaci\u00f3 entre aigua freda, ACS i tractaments t\u00e8rmics.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Clorurs, oxidants, pH i temperatura m\u00e0xima.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Tensions, soldadures, estancament, dip\u00f2sits i escletxes.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Exposici\u00f3 interior, exterior, costanera o industrial.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Risc d&#8217;entrada d&#8217;aigua sota a\u00efllament.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Contingut de sals solubles i pH de l&#8217;a\u00efllament quan resulti aplicable.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 Compatibilitat de r\u00e0cords, juntes i restants components.<\/p>\n\n<p class=\"wp-block-paragraph\">\u2022 L\u00edmits del fabricant de l&#8217;equip i del sistema.<\/p>\n\n<h2 class=\"wp-block-heading\"><strong>Preguntes freq\u00fcents<\/strong><\/h2>\n\n<h3 class=\"wp-block-heading\"><strong>L&#8217;AISI 304 serveix per a aigua potable?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\">S\u00ed, sempre que la refer\u00e8ncia estigui certificada per a aigua de consum i l&#8217;an\u00e0lisi de l&#8217;aigua, la temperatura i el disseny siguin compatibles amb els seus l\u00edmits. En xarxes interiors d&#8217;aigua freda, amb composici\u00f3 ordin\u00e0ria, circulaci\u00f3 adequada i sense exposici\u00f3 exterior a sals, el 304 acostuma a ser suficient. En ACS no s&#8217;ha de traslladar autom\u00e0ticament aquesta conclusi\u00f3: la temperatura m\u00e9s alta, els tractaments t\u00e8rmics, l&#8217;estancament i els dip\u00f2sits redueixen el marge i obligen a revisar les condicions completes.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>Quan conv\u00e9 triar AISI 316L?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\">Conv\u00e9 considerar-ho quan es necessita m\u00e9s marge davant de picadures i corrosi\u00f3 en escletxes per clorurs, existeix exposici\u00f3 exterior a sals, augmenta la temperatura o ho exigeix l&#8217;especificaci\u00f3 del sistema. El seu molibd\u00e8 millora la resist\u00e8ncia relativa davant del 304, per\u00f2 no el fa immune ni elimina la fissuraci\u00f3 per clorurs. La decisi\u00f3 s&#8217;ha de mantenir dins dels l\u00edmits documentats i considerar tamb\u00e9 soldadures, tensions, dip\u00f2sits, a\u00efllament i manteniment.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>L&#8217;AISI 316L \u00e9s apte per transportar aigua de mar?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\"><strong>No s&#8217;ha de considerar universalment apte.<\/strong> L&#8217;aigua de mar cont\u00e9 molts m\u00e9s clorurs que una xarxa potable i el 316L pot patir picadures i corrosi\u00f3 en escletxes, sobre tot amb dip\u00f2sits, estancament o zones geom\u00e8tricament confinades. Una conducci\u00f3 d&#8217;aigua de mar requereix seleccionar espec\u00edficament l&#8217;aliatge, el disseny, les unions, el r\u00e8gim de circulaci\u00f3 i la temperatura. En determinades condicions poden ser necessaris inoxidables m\u00e9s aliats, acers d\u00faplex o altres materials.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>L&#8217;AISI 316L \u00e9s obligatori en aerot\u00e8rmia?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\"><strong>No existeix una obligaci\u00f3 general derivada del nom de l&#8217;aplicaci\u00f3.<\/strong> Un circuit interior, tancat, amb fluid controlat i una refer\u00e8ncia certificada pot ser compatible amb AISI 304. El 316L aporta marge quan concorren clorurs, exposici\u00f3 exterior a sals, temperatures m\u00e9s severes o una prescripci\u00f3 del fabricant. Tamb\u00e9 s&#8217;han de revisar el glicol, l&#8217;aigua de mescla, les unions, l&#8217;a\u00efllament i el manteniment previst durant la vida de la instal\u00b7laci\u00f3.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>El glicol exigeix AISI 316L?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\"><strong>No autom\u00e0ticament.<\/strong> Un glicol nou, correctament formulat i inhibit, pot ser compatible amb diferents materials. La selecci\u00f3 dep\u00e8n del producte comercial, la seva concentraci\u00f3, els inhibidors, l&#8217;aigua utilitzada per mesclar o reposar, la temperatura, l&#8217;oxigen i el manteniment. S&#8217;han de consultar les fitxes del fluid i del sistema. Un canvi de pH, la degradaci\u00f3 del fluid o l&#8217;entrada de contaminants poden modificar la compatibilitat inicialment prevista.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>Qu\u00e8 \u00e9s la corrosi\u00f3 sota tensi\u00f3 per clorurs?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\"><strong>\u00c9s una fissuraci\u00f3 que apareix quan coincideixen clorurs, tensions de tracci\u00f3 i condicions t\u00e8rmiques favorables.<\/strong> En immersi\u00f3 completa i medis aproximadament neutres \u00e9s poc habitual per sota d&#8217;uns 50 \u00b0C, per\u00f2 la concentraci\u00f3 de sals per evaporaci\u00f3 o sota a\u00efllament pot permetre-la a temperatures inferiors. Tant el 304 com el 316L s\u00f3n susceptibles. El molibd\u00e8 del 316L millora altres mecanismes de corrosi\u00f3 localitzada, per\u00f2 no elimina aquest risc.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>Un PREN de 25 significa un 25 % m\u00e9s de resist\u00e8ncia?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\">No. El PREN \u00e9s un \u00edndex calculat a partir del crom, molibd\u00e8 i nitrogen que permet comparar la resist\u00e8ncia relativa a la picadura entre aliatges. No expressa un percentatge de durada, seguretat o vida \u00fatil. Tampoc incorpora temperatura, pH, oxidants, escletxes, dip\u00f2sits, soldadures o tensions. Per completar la comparaci\u00f3 es poden emprar assajos de CPT i CCT, els resultats dels quals tamb\u00e9 s\u00f3n valors de laboratori i no l\u00edmits directes de servei.<\/p>\n\n<h3 class=\"wp-block-heading\"><strong>Qu\u00e8 ha de sol\u00b7licitar l&#8217;instal\u00b7lador abans de triar?<\/strong><\/h3>\n\n<p class=\"wp-block-paragraph\">Ha de disposar de l&#8217;an\u00e0lisi de l&#8217;aigua o la fitxa completa del fluid, temperatures normals i m\u00e0ximes, condicions ambientals, tipus d&#8217;uni\u00f3, a\u00efllament, manteniment i certificacions de la refer\u00e8ncia. En aigua de consum ha de verificar la conformitat del producte complet d&#8217;acord amb el <a href=\"https:\/\/www.boe.es\/buscar\/act.php?id=BOE-A-2023-628\">Real Decreto 3\/2023<\/a>. En ACS ha de considerar les temperatures exigibles i els tractaments t\u00e8rmics. Sense aquestes dades, triar 304 o 316L \u00e9s una prefer\u00e8ncia, no una decisi\u00f3 t\u00e8cnica documentada.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>En una xarxa interior d&#8217;aigua freda potable, amb aigua de composici\u00f3 ordin\u00e0ria i una refer\u00e8ncia certificada, l&#8217;AISI 304 acostuma a ser suficient. L&#8217;AISI 316L aporta un marge addicional quan augmenten els clorurs, la temperatura o l&#8217;exposici\u00f3 exterior a sals, i quan la documentaci\u00f3 del producte o l&#8217;enginyeria del projecte ho prescriu. En aigua calenta sanit\u00e0ria,&hellip;<\/p>\n","protected":false},"author":1,"featured_media":20039,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[267],"tags":[],"class_list":["post-20068","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-tub-corrugat-inox-sistema-cats","category-267","description-off"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v26.9 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas<\/title>\n<meta name=\"description\" content=\"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l&#039;acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\" \/>\n<meta property=\"og:locale\" content=\"ca_ES\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas\" \/>\n<meta property=\"og:description\" content=\"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l&#039;acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\" \/>\n<meta property=\"og:site_name\" content=\"AZ Broquetas\" \/>\n<meta property=\"article:published_time\" content=\"2026-11-06T15:30:19+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2026-11-06T15:41:54+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp\" \/>\n\t<meta property=\"og:image:width\" content=\"1920\" \/>\n\t<meta property=\"og:image:height\" content=\"1080\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/webp\" \/>\n<meta name=\"author\" content=\"Test_A_Admin\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Escrit per\" \/>\n\t<meta name=\"twitter:data1\" content=\"Test_A_Admin\" \/>\n\t<meta name=\"twitter:label2\" content=\"Temps estimat de lectura\" \/>\n\t<meta name=\"twitter:data2\" content=\"15 minuts\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#article\",\"isPartOf\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\"},\"author\":{\"name\":\"Test_A_Admin\",\"@id\":\"https:\/\/az-broquetas.es\/ca#\/schema\/person\/7b11115370891598e3e00508ab129e4f\"},\"headline\":\"Difer\u00e8ncies entre l&#8217;acer inoxidable AISI 304 i l&#8217;AISI 316L: quan triar cada grau\",\"datePublished\":\"2026-11-06T15:30:19+00:00\",\"dateModified\":\"2026-11-06T15:41:54+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\"},\"wordCount\":3173,\"commentCount\":0,\"publisher\":{\"@id\":\"https:\/\/az-broquetas.es\/ca#organization\"},\"image\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage\"},\"thumbnailUrl\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp\",\"articleSection\":[\"Sistemes de canonades CATS\"],\"inLanguage\":\"ca\",\"potentialAction\":[{\"@type\":\"CommentAction\",\"name\":\"Comment\",\"target\":[\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#respond\"]}]},{\"@type\":\"WebPage\",\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\",\"url\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\",\"name\":\"Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas\",\"isPartOf\":{\"@id\":\"https:\/\/az-broquetas.es\/ca#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage\"},\"image\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage\"},\"thumbnailUrl\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp\",\"datePublished\":\"2026-11-06T15:30:19+00:00\",\"dateModified\":\"2026-11-06T15:41:54+00:00\",\"description\":\"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l'acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.\",\"breadcrumb\":{\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#breadcrumb\"},\"inLanguage\":\"ca\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"ca\",\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage\",\"url\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp\",\"contentUrl\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp\",\"width\":1920,\"height\":1080},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Portada\",\"item\":\"https:\/\/az-broquetas.es\/ca\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Difer\u00e8ncies entre l&#8217;acer inoxidable AISI 304 i l&#8217;AISI 316L: quan triar cada grau\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/az-broquetas.es\/ca#website\",\"url\":\"https:\/\/az-broquetas.es\/ca\",\"name\":\"AZ Broquetas\",\"description\":\"Soluciones de conexi\u00f3n innovadoras\",\"publisher\":{\"@id\":\"https:\/\/az-broquetas.es\/ca#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/az-broquetas.es\/ca?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ca\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/az-broquetas.es\/ca#organization\",\"name\":\"AZ Broquetas\",\"url\":\"https:\/\/az-broquetas.es\/ca\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ca\",\"@id\":\"https:\/\/az-broquetas.es\/ca#\/schema\/logo\/image\/\",\"url\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2024\/03\/Logo-AZ.png\",\"contentUrl\":\"https:\/\/az-broquetas.es\/wp-content\/uploads\/2024\/03\/Logo-AZ.png\",\"width\":350,\"height\":100,\"caption\":\"AZ Broquetas\"},\"image\":{\"@id\":\"https:\/\/az-broquetas.es\/ca#\/schema\/logo\/image\/\"},\"sameAs\":[\"https:\/\/www.linkedin.com\/company\/az-broquetas-s-l\/\",\"https:\/\/www.youtube.com\/@azbroquetass.l7674\"]},{\"@type\":\"Person\",\"@id\":\"https:\/\/az-broquetas.es\/ca#\/schema\/person\/7b11115370891598e3e00508ab129e4f\",\"name\":\"Test_A_Admin\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ca\",\"@id\":\"https:\/\/az-broquetas.es\/ca#\/schema\/person\/image\/\",\"url\":\"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g\",\"contentUrl\":\"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g\",\"caption\":\"Test_A_Admin\"},\"sameAs\":[\"https:\/\/az-broquetas.es\"]}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas","description":"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l'acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","og_locale":"ca_ES","og_type":"article","og_title":"Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas","og_description":"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l'acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.","og_url":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","og_site_name":"AZ Broquetas","article_published_time":"2026-11-06T15:30:19+00:00","article_modified_time":"2026-11-06T15:41:54+00:00","og_image":[{"width":1920,"height":1080,"url":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp","type":"image\/webp"}],"author":"Test_A_Admin","twitter_card":"summary_large_image","twitter_misc":{"Escrit per":"Test_A_Admin","Temps estimat de lectura":"15 minuts"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#article","isPartOf":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau"},"author":{"name":"Test_A_Admin","@id":"https:\/\/az-broquetas.es\/ca#\/schema\/person\/7b11115370891598e3e00508ab129e4f"},"headline":"Difer\u00e8ncies entre l&#8217;acer inoxidable AISI 304 i l&#8217;AISI 316L: quan triar cada grau","datePublished":"2026-11-06T15:30:19+00:00","dateModified":"2026-11-06T15:41:54+00:00","mainEntityOfPage":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau"},"wordCount":3173,"commentCount":0,"publisher":{"@id":"https:\/\/az-broquetas.es\/ca#organization"},"image":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage"},"thumbnailUrl":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp","articleSection":["Sistemes de canonades CATS"],"inLanguage":"ca","potentialAction":[{"@type":"CommentAction","name":"Comment","target":["https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#respond"]}]},{"@type":"WebPage","@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","url":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau","name":"Difer\u00e8ncies entre acer inoxidable AISI 304 i 316L - AZ Broquetas","isPartOf":{"@id":"https:\/\/az-broquetas.es\/ca#website"},"primaryImageOfPage":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage"},"image":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage"},"thumbnailUrl":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp","datePublished":"2026-11-06T15:30:19+00:00","dateModified":"2026-11-06T15:41:54+00:00","description":"Difer\u00e8ncies entre AISI 304 i 316L i criteris per triar l'acer inoxidable segons clorurs, temperatura, ambient, soldadura i aplicaci\u00f3.","breadcrumb":{"@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#breadcrumb"},"inLanguage":"ca","potentialAction":[{"@type":"ReadAction","target":["https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau"]}]},{"@type":"ImageObject","inLanguage":"ca","@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#primaryimage","url":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp","contentUrl":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2026\/10\/diferencias-acero-inoxidable-316l-y-acero-inoxidable-304.webp","width":1920,"height":1080},{"@type":"BreadcrumbList","@id":"https:\/\/az-broquetas.es\/ca\/diferencies-entre-lacer-inoxidable-aisi-304-i-laisi-316l-quan-triar-cada-grau#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Portada","item":"https:\/\/az-broquetas.es\/ca"},{"@type":"ListItem","position":2,"name":"Difer\u00e8ncies entre l&#8217;acer inoxidable AISI 304 i l&#8217;AISI 316L: quan triar cada grau"}]},{"@type":"WebSite","@id":"https:\/\/az-broquetas.es\/ca#website","url":"https:\/\/az-broquetas.es\/ca","name":"AZ Broquetas","description":"Soluciones de conexi\u00f3n innovadoras","publisher":{"@id":"https:\/\/az-broquetas.es\/ca#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/az-broquetas.es\/ca?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ca"},{"@type":"Organization","@id":"https:\/\/az-broquetas.es\/ca#organization","name":"AZ Broquetas","url":"https:\/\/az-broquetas.es\/ca","logo":{"@type":"ImageObject","inLanguage":"ca","@id":"https:\/\/az-broquetas.es\/ca#\/schema\/logo\/image\/","url":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2024\/03\/Logo-AZ.png","contentUrl":"https:\/\/az-broquetas.es\/wp-content\/uploads\/2024\/03\/Logo-AZ.png","width":350,"height":100,"caption":"AZ Broquetas"},"image":{"@id":"https:\/\/az-broquetas.es\/ca#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.linkedin.com\/company\/az-broquetas-s-l\/","https:\/\/www.youtube.com\/@azbroquetass.l7674"]},{"@type":"Person","@id":"https:\/\/az-broquetas.es\/ca#\/schema\/person\/7b11115370891598e3e00508ab129e4f","name":"Test_A_Admin","image":{"@type":"ImageObject","inLanguage":"ca","@id":"https:\/\/az-broquetas.es\/ca#\/schema\/person\/image\/","url":"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g","caption":"Test_A_Admin"},"sameAs":["https:\/\/az-broquetas.es"]}]}},"_links":{"self":[{"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/posts\/20068","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/comments?post=20068"}],"version-history":[{"count":2,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/posts\/20068\/revisions"}],"predecessor-version":[{"id":20088,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/posts\/20068\/revisions\/20088"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/media\/20039"}],"wp:attachment":[{"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/media?parent=20068"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/categories?post=20068"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/az-broquetas.es\/ca\/wp-json\/wp\/v2\/tags?post=20068"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}